Heat Treatment And Coating Line
Zinc-Aluminum-Magnesium Coating Production Line(Meeting the latest zinc-aluminum-magnesium coating process requirements)
View product category, application direction, and core equipment information.
Technical Data
Process Range And Operating Parameters
| Processing Material | High carbon steel wire (carbon content: 0.77-0.97%),82B、82MnSi、87MnSi、 92Si、97Si |
| Wire Diameter Range | Ø4.0mm - Ø8.0mm |
| Number of Processing Lines | 12/16/20 According to customer requirements |
| Process Speed | DV 150 mm*m/min |
| Process Flow | 1250Wire reel pay-off → straightening → high-temperaturedegreasing → electrolytic alkaline cleaning → three-stagewater cleaning → smoke-free pickling → three-stagewater cleaning → fluxing → drying → hot-dip galvanizing → fluxing(Galfan-2m) → drying(Galfan-5m) → hot-dipGalfan → 900 dual‑drum traction machine + 1250 spool take‑up |
| Technical Specifications | Stable and adjustable wire tension; hot-dip galvanizing,usingnitrogen/press blockwiping;zinc coating weight190-350g/㎡,GalfancoatingComplies withGB/T20492-2019 AClassstandard |
| Pay-off Mode | 1250wire reelContinuous pay-off(double drum accumulation,Coil change without stopping) |
| Take-up Mode | 1250wire reelContinuous take-up(double drum accumulation,Coil change without stopping) |
| Electrical Control | Single wireindependent control、Variable frequency drive、PLCcontrol、Full-process control with process parameter setting and display |